ASTM E140 conversion (non-austenitic steels)
| HRC | HV | HB (carbide ball) |
|---|---|---|
| 68 | 940 | – |
| 66 | 865 | – |
| 64 | 800 | 722 |
| 62 | 746 | 688 |
| 60 | 697 | 654 |
| 58 | 653 | 615 |
| 56 | 613 | 577 |
| 54 | 577 | 543 |
| 52 | 544 | 512 |
| 50 | 513 | 481 |
| 48 | 484 | 455 |
| 46 | 458 | 432 |
| 44 | 434 | 409 |
| 42 | 412 | 390 |
| 40 | 392 | 371 |
| 38 | 372 | 353 |
| 36 | 354 | 336 |
| 34 | 336 | 319 |
| 32 | 318 | 301 |
| 30 | 302 | 286 |
| 28 | 286 | 271 |
| 26 | 272 | 258 |
| 24 | 260 | 247 |
| 22 | 248 | 237 |
| 20 | 238 | 226 |
Values from ASTM E140 Table 1 (Rockwell C range). Brinell values use a 10 mm tungsten carbide ball and 3,000 kgf load.
Accuracy
Hardness scales measure different things, so conversions are approximate and only valid for the material the table was built from: carbon and alloy steels that aren't austenitic. Stainless steels, cast iron, aluminium and copper alloys have their own tables. For specifications, test in the scale the specification calls for.
Tensile strength ≈ 3.45 × HB (MPa), a widely used rule of thumb for steels
Tips
- Typical values: mild steel about HRC 10–20 (below this table), hardened tool steel HRC 58–64, knife blades HRC 55–62.
- For stresses, see the von Mises stress calculator; for strength checks, the beam deflection calculator.
Frequently asked questions
What is HRC 60 in Vickers?
About 697 HV.
What is HRC 50 in Brinell?
About 481 HB with a carbide ball.
Can I convert stainless steel hardness with this?
No; austenitic stainless steels need their own conversion table.
Written and checked by Vijay. Last updated .